LLS-09 Ant Repellent (Low Smoke Halogen-Free, for PVC)
Contact Info
- Add:辽宁省鞍山市海城市腾鳌镇寿安街道, Zip:
- Contact: 朱闻雷
- Tel:13905772710
- Email:leilikj@163.com
Other Products
The LLS-09 termiticide product developed by our company is primarily composed of a mixture of various pyrethroids, carbamates, and other compounds. It appears as a white powder with a melting point of 86-90°C and a decomposition temperature ≥200°C. It is stable under light and heat. This product has passed the EU ROHS Directive test and the SVHC (Substances of Very High Concern) inspection. It is non-"three-genetic" (carcinogenic, teratogenic, mutagenic) to humans, making it a medium-to-low toxicity, highly efficient, and long half-life termiticide with strong contact-killing action, rapid knockdown power, and quick efficacy. It is particularly effective in controlling termites and is widely used in PVC and low-smoke zero-halogen plastic sheathing. Recommended dosage: 0.6-1.0%.
Precautions:
1. As the LLS-09 termiticide product has a certain level of toxicity, protective measures should be taken during use.
2. If it comes into contact with the skin, wash thoroughly with soap and water.
Storage:
The product should be stored sealed in a cool, dry, and well-ventilated place.
The "termite-resistant PVC sheathing plastic" made with this product, when tested according to JB/T 10696.9-2011 (Test Methods for Mechanical and Physicochemical Properties of Electric Cables and Wires - Part 9: Termite Test), meets the Kt50 min value standards for various sheathing materials.
The mechanical performance test results of the termite-resistant PVC sheathing plastic are as follows:
|
Test Item |
Standard Requirement |
Measured Result |
Individual Conclusion |
|
1. Mechanical Properties Before Aging - Tensile Strength (N/mm2) |
≥12.5 |
19.7 |
Qualified |
|
Elongation at Break (%) |
≥150 |
300 |
Qualified |
|
2. After Air Oven Aging |
|||
|
Temperature (°C) 100±2, Time (h) 168 |
|||
|
Tensile Strength (N/mm2) |
≥12.5 |
21.7 |
Qualified |
|
Change Rate (%) |
≤±25 |
+9.7 |
Qualified |
|
Elongation at Break (%) |
≥150 |
350 |
Qualified |
|
Change Rate (%) |
≤±25 |
16.6 |
Qualified |
|
3. Thermal Weight Loss Test |
|||
|
Temperature (°C) 80±2, Time (h) 168 |
|||
|
Weight Loss (%) |
≤2.0 |
0.34 |
Qualified |
|
4. Anti-Cracking Test |
|||
|
Temperature (°C) -, Time (h) - |
|||
|
Test Result |
No Cracking |
No Cracking |
Qualified |
|
5. High Temperature Pressure Resistance Test |
|||
|
Temperature (°C) 80±2, Time (h) 4 |
|||
|
Deformation Rate (%) |
≤50 |
22 |
Qualified |
|
6. Low Temperature Impact Test |
|||
|
Temperature (°C) -15±2 |
|||
|
Test Result |
No Cracking |
No Cracking |
Qualified |
The extrusion process is stable, with fast wire output speed, uniform plasticization, smooth surface, no visible pores by visual inspection, and no odor.